Special Tip:
NARA CERAMIC CLAY should be kept in an airtight
storage in order to remain soft.
- Recommendation for using :
Knead and shape. - A finished product needs to dry up
within 24 hours on open air in a normal temperature without shrinking or bending. - The finished product can be painted and vanished.
- To get porcelain, it must be fired at 1,000-1,300 °C(or 2,012-2,192 °F).